Parts exhibit high tensile, fatigue, creep, and rupture strength at temperatures up to 850°C (1560°F), along with outstanding corrosion and oxidation resistance. They remain crack-free in both as-manufactured and heat-treated conditions and are resistant to strain-age cracking. A short, AM-optimized heat treatment is required, but no hot isostatic pressing (HIP) is needed.

Recent Posts
  • admin_eds
  • November 11, 2024

EOS NickelAlloy IN939

Parts exhibit high tensile, fatigue, creep, and rupture strength at temperatures up to 850°C (1560°F), along with outstanding corrosion and oxidation resistance. They remain crack-free in both as-manufactured and heat-treated conditions and are resistant to strain-age cracking. A short, AM-optimized heat treatment is required, but no hot isostatic pressing (HIP) is needed.